Drolith MS500
Moisture-control additive
Molecular sieve dispersion in castor oil used as a moisture scavenger in Drothane formulations.
PU coatings · Sealants
- Solids concentration
- 48 - 52%
- Viscosity @ 25°C (Brookfield)
- < 18000cP; ASTM D 2196
Activated molecular sieve 3A powder used as a moisture scavenger.
An activated molecular-sieve powder for moisture control in one- or two-component PU coatings and adhesives.
Read every value with its unit and test conditions.
Source: TDS, 25th June, 2026 Ver.- 2. Values and test methods are as stated in this TDS.
| Property | Value / range | Unit & test conditions |
|---|---|---|
| Static H2O Adsorption @15%RH & 30°C | > 22 | % wt. |
| Static H2O Adsorption @75%RH & 30°C | > 25 | % wt. |
| Loss on drying @ 350°C | < 2 | % wt. |
| Particle Size | 3 - 6 mic | d max |
| pH value | < 11 | ~ |