Dromal 2351
Rosin-modified maleic resin
Rosin-modified maleic resin with a penta-ester-based composition.
Printing inks · Coatings
- Melting point
- 120 - 130°C; ISO 11357 - 3
- Flow time @ 30°C by FC B4 (50% solution in toluene)
- 20 - 30s; ASTM D 2196
Rosin-modified maleic resin with a glycerol-based composition.
A glycerol-based, rosin-modified maleic resin candidate for inks and coatings.
| Component / property | Dromal 2352This grade | Dromal 2353with vergleichen |
|---|---|---|
| Component | Rosin-modified maleic resin | Rosin-modified maleic resin |
| Listed uses | Printing inks; Coatings | Printing inks; Coatings |
| Melting point°C; ISO 11357 - 3 | 110 - 130 | 120 - 135 |
| Acid valuemg KOH/g; ASTM D 1980-87 | 30 max | 145 max |
Read every value with its unit and test conditions.
Source: TDS, 17th October, 2022 Ver.- 1.1. Values and test methods are as stated in this TDS.
| Property | Value / range | Unit & test conditions |
|---|---|---|
| Appearance | Yellow to dark brown brittle lumps | Visual |
| Color (50% solution in toluene) | 12 max | CGS; ASTM D 1544 |
| Acid value | 30 max | mg KOH/g; ASTM D 1980-87 |
| Flow time @ 30°C by FC B4 (50% solution in toluene) | 15 - 20 | s; ASTM D 2196 |
| Melting point | 110 - 130 | °C; ISO 11357 - 3 |
How to read technical properties · Evaluate the complete formulation in your intended process.